【Member Papers】Single pulse laser induced crystallization and defect engineer of Ga₂O₃ film for achieving high performance solar blind photodetector

日期:2026-11-26阅读:48

      Researchers from the Xiamen Key Laboratory of Development and Application for Advanced Semiconductor Coating Technology, School of Opto-electronic and Communication Engineering, Xiamen University of Technology, Xiamen, China, and the School of Electrical and Information Engineering, North Minzu University, Yinchuan, Ningxia, China have published a research article titled " Single-pulse laser-induced crystallization and defect engineer of Ga₂O₃ film for achieving high-performance solar-blind photodetector" in Surface & Coatings Technology.

 

Background

      Gallium oxide (Ga₂O₃) is an ultra‑wide‑bandgap semiconductor with a bandgap of 4.8–5.3 eV, exhibits a high critical electric field as well as robust chemical and thermal stability. These favorable properties render Ga₂O₃ attractive for diverse applications, including high‑power electronics, radiation detection, gas sensing, and solar‑blind photodetectors (SBPDs). The solar‑blind region from 200 to 280 nm in sunlight rarely reaches the Earth's surface because of strong absorption by the atmosphere, which enables SBPDs with high anti‑interference, high photosensitivity, and high reliability. The absorption region of Ga₂O₃ is located within the solar‑blind region with high photon absorption efficiency. Therefore, Ga₂O₃ is one of the most desirable candidates for the fabrication of high‑performance SBPDs, which are suitable for applications in flame monitoring, ultraviolet imaging, environmental sensing, and space communication. However, high‑performance Ga₂O₃ SBPDs face a fundamental trade‑off between responsivity and response speed. The trap states in Ga₂O₃, especially oxygen vacancies, can prolong the photogenerated‑carrier lifetime thereby slowing the response and increasing the dark current. Meanwhile, they also can increase photoconductive gain resulting in high responsivity. Therefore, simultaneously achieving high photoresponsivity, low dark current, and fast response remains a challenge. Several approaches, including annealing, doping, and surface passivation, have been used to regulate oxygen vacancies. However, reducing bulk defects generally improves response speed at the cost of photoconductive gain. Nevertheless, the high growth temperature or prolonged high‑temperature post‑annealing is generally required to achieve a high‑quality upper layer resulting in a high thermal budget. Besides, those processes may also partially repair defects in the underlying gain layer, thereby reducing photoconductive gain. Laser annealing offers a potential solution because its localized, short‑duration high‑temperature heating can selectively crystallize and repair defects near the irradiated surface while limiting thermal effects on deeper layers and the substrate. To date, the studies on laser‑annealed Ga₂O₃ films are seldom. Moreover, studies employing laser annealing to regulate oxygen vacancies in high‑performance Ga₂O₃ SBPDs remain scarce.

 

Highlights

      1.Low-thermal-budget fluence-dependent controllable crystallization of amorphous Ga₂O₃: The team annealed a ~200 nm room-temperature-deposited amorphous Ga₂O₃ film using a 248 nm, 20 ns single-pulse excimer laser without prolonged high-temperature treatment. Monoclinic β-Ga₂O₃ emerges at 400 mJ/cm²; higher fluence promotes grain growth and broadens the optical bandgap from 4.82 eV to 5.12 eV .

      2.Simulation combined with characterization clarifies the oxygen-vacancy gradient mechanism: Thermal-transport simulation reveals a steep in-depth temperature gradient and fluence-dependent melting depth (15-180 nm for 400-600 mJ/cm²). Depth-resolved XPS verifies an intrinsic oxygen-vacancy gradient with increasing vacancy concentration from surface to interior for the 500 mJ/cm²-annealed film, where the OV/(OL + OV) ratio increases from 5.04% at 4 min etching to 18.78% at 16 min etching .

      3.Gradient defects balance the responsivity and spond speed: Low surface oxygen-vacancy concentration suppresses dark leakage while the vacancy-rich inner layer preserves photoconductive gain..

      4.High-speed, high-performance MSM solar-blind photodetector: The MSM device based on the 500 mJ/cm²-annealed film obtains a dark current of 1.14 × 10⁻¹² A, a photo-to-dark current ratio of 3.23 × 10⁶, and a specific detectivity of 1.13 × 10¹⁵ Jones. The rise/decay time reduces from 4.11/0.22 s to 0.05/0.02 s with excellent solar-blind selectivity (R₂₅₄/R₄₀₀ of 2.06 × 10⁵).

 

Conclusion

      In this study, single-pulse laser annealing (SPLA) was demonstrated as an effectively low thermal-budget route for crystallizing and defect-engineering Ga₂O₃ thin films and was applied to SBPDs. Raising the laser energy density from 300 to 600 mJ/cm² resulted in a progressive widening of the Ga₂O₃ bandgap. The amorphous Ga₂O₃ films began to crystallize at 400 mJ/cm², and crystallization was further enhanced with the increasing laser energy density because greater energy input increased atomic diffusion and the driving force for nucleation and grain coarsening. However, excessive energy input caused substantial grain agglomeration and surface roughening, as evidenced by the sharp increase in RMS roughness for the film annealed at 600 mJ/cm².

      Thermal-transport simulations of SPLA were conducted and revealed the pronounced temperature gradient through the film depth. The temperature gradient plays a key role in the depth-dependent defect distribution in Ga₂O₃ film, which has been verified by the depth-resolved XPS. The gradient distribution of oxygen-vacancy defects can effectively suppress leakage current while preserving sufficient photoconductive gain. Finally, the MSM SBPD based on the film annealed at 500 mJ/cm² achieved the best overall performance, including a low Idark of 1.14 × 10⁻¹² A, a high PDCR of 3.23 × 10⁶, a high R of 46.51 A/W, a high D* of 1.13 × 10¹⁵ Jones, and a tr/td values of 0.05/0.02 s at a bias of 5 V. Hence, SPLA may offer a viable strategy for balancing the responsivity and response speed in high-performance Ga₂O₃ SBPDs.

 

Fig. 1. Optical properties of Ga₂O₃ thin films before and after laser annealing at different energy densities: (a) transmittance spectra, with the inset showing the Tauc plots, and (b) optical bandgaps.

Fig. 2. Structural properties of Ga₂O₃ thin films before and after laser annealing at different laser energy densities: (a) XRD patterns and (b) crystallite sizes and microstrain.

Fig. 3. Top‑view FESEM images of Ga₂O₃ thin films before and after laser annealing at different energy densities: (a) as‑grown, (b) 300 mJ/cm², (c) 400 mJ/cm², (d) 500 mJ/cm², (e) 600 mJ/cm², the inset shows particle size distribution analysis, and (f) average particle size.

Fig. 4. Three‑dimensional AFM images of Ga₂O₃ films before and after laser annealing at different energy densities: (a) as‑grown, (b) 300 mJ/cm², (c) 400 mJ/cm², (d) 500 mJ/cm² (e) 600 mJ/cm², and (f) RMS roughness.

Fig. 5. Thermal‑field simulation of SPLA at various energy densities: (a) schematic of the simulation geometry, (b) surface temperature as a function of time, (c) maximum temperature as a function of depth, and (d) melting depth and melting duration versus energy density.

Fig. 6. XPS depth profiles of Ga₂O₃ films after 500 mJ/cm² laser annealing: (a) survey spectra and (b) atomic ratios of Ga, O, and C.

Fig. 7. High-resolution Ga 3d spectra of Ga₂O₃ thin films after laser annealing at 500 mJ/cm² and subsequent Ar⁺ ion etching for (a) 4 min, (b) 8 min, (c) 12 min, and (d) 16 min. (e) Relative peak-area fractions of the Ga³⁺ and Ga⁺ components as a function of etching time.

Fig. 8. High‑resolution O 1 s spectra of Ga₂O₃ thin films after laser annealing at 500 mJ/cm² and subsequent Ar⁺ ion etching for (a) 4 min, (b) 8 min, (c) 12 min, and (d) 16 min. (e) Oᵥ/(OL+Oᵥ) ratios as a function of etching time.

Fig. 9. Schematic illustration of the laser‑annealing mechanism and simulated temperature‑depth distributions of Ga₂O₃ thin films: (a) as‑grown, (b) 300 mJ/cm², (c) 500 mJ/cm², and (d) 600 mJ/cm².

Fig. 10. (a) Schematic structure and (b) top‑view optical micrograph of Ga₂O₃ MSM PDs. (c) I‑V characteristics under dark and 254 nm UV light illumination. (d) I‑t curves, (e) responsivity spectra and (f) UV‑to‑visible rejection ratio (R₂₅₄/R₄₀₀) of PDs based on films annealed at different energy densities. (g) Transient photoresponse under various UV light power densities and (h) Iphoto versus P of the PD based on the Ga₂O₃ film annealed at 500 mJ/cm².

 

DOI:

10.1016/j.surfcoat.2026.134099