【Domestic Papers】Defect compensation and recombination characteristics of NiO/β-Ga₂O₃ heterojunctions under electronic-stopping-dominated swift heavy-ion irradiation
日期:2026-11-26阅读:45
Researchers from the Nanjing University have published a dissertation titled "Defect compensation and recombination characteristics of NiO/β-Ga₂O₃ heterojunctions under electronic-stopping-dominated swift heavy-ion irradiation" in Applied Physics Letters.
Background
Gallium oxide (β-Ga₂O₃) has emerged as a promising ultrawide-bandgap semiconductor for next-generation power electronics owing to its large bandgap (~4.8 eV), high critical breakdown field, and superior Baliga’s figure of merit (BFOM). Its high threshold displacement energy also makes β-Ga₂O₃ attractive for extreme irradiation environments such as aerospace and deep-space platforms. However, carrier transport in β-Ga₂O₃ devices is sensitive to deep-level defects introduced during growth, fabrication, or energetic-particle irradiation. In particular, near-interface deep-level traps can modify junction electrostatics and activate field-assisted recombination pathways beyond the conventional Shockley–Read–Hall (SRH) transport framework. Understanding how energetic-ion irradiation modifies these recombination-active traps is essential for evaluating device reliability.
Abstract
Understanding how irradiation influences recombination-active defects and carrier transport is crucial for establishing the radiation tolerance of Ga2O3 power electronics. Here, we investigate the effects of 1.86 GeV 181Ta31+ swift heavy-ion irradiation on NiO/β-Ga2O3 heterojunction power diodes. Capacitance profiling reveals a pronounced near-surface carrier-removal rate of 9.2 × 107 cm−1 on the β-Ga2O3 side, indicating partial donor compensation in the depletion region. Deep-level transient spectroscopy further reveals irradiation-induced compensation of electrically active defects, in which the E2-related traps (EC-0.818 eV) are no longer resolved within the investigated temperature range, while E2* traps shift deeper from EC-0.670 to EC-0.733 eV and bulk-distributed E9 traps (EC-0.392 eV) remain nearly unchanged. Correspondingly, the subthreshold forward-bias transport behavior changes from tunneling-assisted recombination with a peak ideality factor (η) of 20.75 to a conventional Shockley–Read–Hall recombination mechanism (η≈2) after irradiation, whereas the reverse transport characteristics remain largely consistent with Poole–Frenkel emission with a nearly unchanged activation energy. These results suggest that electronic-stopping-dominated irradiation is accompanied by the compensation of electrically active defects and enhanced carrier compensation within the depletion region, which are associated with the observed changes in the dominant recombination behavior of β-Ga2O3 heterojunction devices under the present irradiation condition.
Highlights
Following irradiation with 1.86 GeV Ta fast heavy ions, the near-surface carrier removal rate in β-Ga₂O₃ reached 9.2 × 10⁷ cm⁻¹, indicating significant carrier compensation within the depletion zone.
Following irradiation, the E2-related trap signal was no longer observed within the tested temperature range; forward subthreshold transport changed from tunnelling-assisted recombination to conventional SRH recombination, whilst reverse transport continued to conform primarily to the Poole–Frenkel emission mechanism.
The E2′ trap energy level deepened from 0.670 eV to 0.733 eV relative to the bottom of the conduction band, whilst the E9 trap remained essentially stable, indicating that irradiation has markedly different effects on different electroactive defects.
Conclusion
In summary, we systematically investigated the impact of GeV-range swift heavy-ion irradiation on defect evolution and carrier transport in NiO/β-Ga₂O₃ heterojunction diodes. Electrical and spectroscopic analyses suggest that irradiation is accompanied by the compensation of electrically active defects, which is associated with the observed changes in the electrical transport characteristics. The observed compensation of E2-related defect, together with irradiation-induced carrier removal, are associated with the suppression of tunneling-assisted recombination and the transition from modified SRH recombination to conventional SRH recombination under forward bias. In contrast, the reverse transport characteristics exhibit comparatively smaller irradiation-induced changes. These results suggest that electronic-stopping-dominated irradiation is accompanied by the compensation of electrically active defects and corresponding changes in the dominant recombination behavior of NiO/β-Ga₂O₃ heterojunctions under the present irradiation condition. Further structural characterization and systematic irradiation studies over a wider range of irradiation conditions will be valuable for clarifying the underlying microscopic mechanisms and their relationship to carrier transport.

FIG. 1. (a) C–V and 1/C2 –V characteristics of the NiO/β-Ga2O3 HJD before and after irradiation. (b) Carrier depth profiles in β-Ga2O3 epilayer extracted from C–V analysis; insets show the cross-sectional schematic of the vertical NiO/β-Ga2O3 HJD. (c) and (d) Temperature-dependent forward J–V characteristics of the HJD measured from 200 to 450 K before and after irradiation, respectively. The blue solid lines represent fitting using the modified SRH recombination model, while the red dashed lines correspond to conventional SRH recombination fitting.

FIG. 2. (a) and (b) Extracted ideality factor η as a function of forward bias at varied temperatures for the pre-irradiation HJD and post-irradiation one. (c) Temperature dependence of the characteristic tunneling parameter E0 extracted from modified SRH fitting. (d) Arrhenius plot of the recombination current Jr for the pre-irradiation HJD, yielding an activation energy Ea of 0.82 6 0.02 eV.

FIG. 3. (a) Reverse J–V characteristics of both devices measured from 200 to 500 K. (b) Temperature-dependent ln(J/E) vs E1/2 characteristics showing linear PF emission behavior at high electric fields. (c) and (d) Arrhenius plots of fitting parameters m(T) and n(T), yielding the high-frequency dielectric permittivity ε∞ and the trap barrier height ΦT, respectively.

FIG. 4. (a) DLTS spectra of the HJDs before and after irradiation, recorded under the condition of VR=−3/−1 V, VP=1.5 V, f=33 Hz, and tP=0.5ms. (b) Arrhenius plots of the extracted trap levels compared with reported defect levels from Dawe et al.25 (E9), Zhang et al.26 (E1), and Ingebrigtsen et al.27 (E2 and E2*). Blue and red dashed lines represent the Arrhenius fits before and after irradiation, respectively. Filled and open symbols denote the extracted and reported trap levels, respectively, showing good agreement.

FIG. 5. Energy-band diagrams, trap spatial distribution, and dominant recombination pathways in the NiO/β-Ga2O3 heterojunction under low forward bias (a) before and (b) after irradiation, illustrating the transition from tunneling-assisted recombination mediated by near-interface E2 traps to conventional SRH recombination dominated by bulk defects following irradiation-induced near-interface defect suppression and carrier removal.
DOI:
doi.org/10.1063/5.0340364